Styrene Impurities on Stabilwax

ColumnStabilwax, 30 m, 0.53 mm ID, 0.50 µm (cat.# 10640)
Sample95% pure styrene
Injection
Inj. Vol.:0.5 µL split
Inj. Temp.:150 °C
Split Vent Flow Rate:40 mL/min
Oven
Oven Temp.:40 °C (hold 10 min) to 150 °C at 10 °C/min (hold 15 min)
Carrier GasHe, constant pressure
Linear Velocity:20 cm/sec @ 40 °C
DetectorFID @ 150 °C
NotesFID sensitivity: 16 x 10-11 AFS
AcknowledgementPermission to publish this chromatogram granted by Copolymer Rubber and Chemical Corp.